Features:
1. Different material is available according to the corrosion characteristics.
2. Different heat treatment process
......................................................................................................................................................................................
Material performance table
| CODE | INSTRUCTION | HARDNESS | MATERIAL |
| A1 | Stainless steel | Ball: HRC 58-65 | UNS 41000–UNS 44000 |
| Seat: HRC 52-56 | 9Cr18Mo & 6 Cr18Mo | ||
| B1 | Cobalt alloy casting | Ball: HRC 56-63 | Cobalt, chromium and tungsten alloy |
| Seat: HRC 50-56 | |||
| B2 |
Cobalt alloy, powder metallurgy |
Ball: HRC 53-60 | Cobalt, chromium and tungsten alloy |
| Seat: HRC 51-57 | |||
| C1 | Tungsten carbide | Ball: HRA 88-89 | Tungsten with cobalt adhesive |
| Seat: HRA 88-89.5 | |||
| C3 | Titanium carbon compounds | Ball: HRA 89-90.5 |
Tungsten and titanium with cobalt adhesive carbon compounds |
| Seat: HRA 89-90.5 |
Size Table:

Finished Product

Raw Material

Inspection

Package